Ring-opening polymerizations of γ-glycidoxypropyltrimethoxysilane (GPTMS) were carried out by using multi-metal cyanide (MMC) catalyst and the synthesized homopolymer was a comb-shaped polymer with regular structure. The structure of the polymer obtained (P-GPTMS) was characterized by FTIR, 1H-NMR, and 29Si-NMR spectroscopy, and the molecular weight and its distribution were analyzed by size-exclusion chromatography with multi-angle laser light scattering (SEC-MALLS). The thermal behavior of P-GPTMS was investigated by differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). P-GPTMS with high molecular weight (Mn = 18,000–80,000) and narrow molecular weight distribution (1.10–1.35) were synthesized when the dosage of MMC catalyst was 0.1% and polymerization temperature was 130 °C. The molecular weight of the product could be adjusted by controlling the polymerization time. The Tg of P-GPTMS is in the range of −34 to −30 °C. On the basis of the TGA data, the decomposition rate of P-GPTMS reached its peak at 374.14 °C and the entire decomposition stopped at 600 °C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.