Abstract

ABSTRACT High carbon steels are employed for the production of critical components, such as ropes, cables and springs. After hot rolling, their microstructure is controlled by Stelmor cooling, since they are often subjected to strong drawing operations. The as-rolled deformability is a basic property to prevent damages in the following plastic deformation. In the industrial world, it is known that their deformability improves significantly after a storage of a certain time, ranging from some days up to 15–20 days. In this experimental work, the deformability of a high carbon steel was investigated after different storage times varying the wire rod diameter. The percentage reduction of area (ROA) increased after some days until a stable value was reached after about 7–15 days depending on the considered diameter. The fracture surfaces of the aged specimens were analysed by SEM.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.