The effect of limewater on flexural strength and water permeability of TiO2 nanoparticles binary blended concrete has been investigated. TiO2 nanoparticles with partial replacement of cement by 0.5, 1.0, 1.5 and 2.0 weight percent have been used as reinforcement. Curing of the specimens has been carried out in water and saturated limewater for 7, 28 and 90 days after casting. The results indicate that TiO2 nanoparticles up to maximum replacement level of 2.0% produces concrete with improved flexural strength and water permeability when the specimens cured in saturated limewater with respect to the specimens cured in water. TiO2 nanoparticles can improve the filler effect and also the high pozzolanic action of fine particles increases substantially the quantity of strengthening gel. Although the limewater curing medium could not improve the compressive strength of concrete with respect to the water curing medium, incorporating nanoparticles could cause more strength and resistance to water permeability for the specimens cured in saturated limewater with respect to the specimens cured in water.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.