Abstract

Wetting by fouling is phenomenon specific to membrane distillation (MD) and are regarded as challenges to the seawater membrane distillation (SWMD) process. To understand fouling and wetting, the influence of Mg and Sr crystals, which can potentially cause scaling, as well as Ca crystals deposited on the membrane surface were investigated. Mg(OH)2 and CaSO4 had significant impact on fouling and wetting. Even if CaCO3 and SrSO4 had no effects on fouling and wetting as single salts, CaCO3 and CaSO4 were dominant in synthetic seawater without Mg(OH)2. However, the occurrence of Mg(OH)2 scales became a cause for concern if Ca ion was removed from seawater for the prevention of fouling and wetting. Therefore, Mg as well as Ca should be removed for proper fouling and wetting control. NaOH/Na2CO3 softening was used for the removal of Ca and Mg ions. In addition, based on the inhibition effects of Mg ions on Ca scales, a new pretreatment method involving the injection of MgCl2 to increase the Mg /Ca ratio was examined.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.