Abstract

A theory based on Grambow`s work on hydration of glass as linear function of solution composition was evaluated. Use of Grambow`s linear rate law for correlation of durability with glass composition is not recommended. Dissolution rate of the glass was determined using the rate of release of sodium with an ion selective electrode. This method was tested first applying it to initial dissolution rate of several glasses at several temperatures with zero initial concentration of silicic acid. HW39-2, HW39-4, and SRL-202 from Savannah River were tested; there was significant scatter in the data, with the dissolution rates of HW39 glasses and the SRL glass being comparable within this scatter. The dissolution rate of SRL-202 at 80 C and pH 7 for silicic acid concentrations 0, 25, 50, and 100% saturation, was found to decrease dramatically at only 25% of the saturated silicic acid concentration, which does not conform to the linear theory.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.