In the article presented are the results of post-irradiation tests of helium bonded fuel pins with mixed mononitride fuel (U0.55Pu0.45)N and (U0.4Pu0.6)N having 85% density irradiated in BOR-60 reactor. Achieved maximum burn-up was, respectively, equal to 9.4 and 12.1 at.% with max linear heat rates 41.9 and 54.5 kW/m. Maximum irradiation dose was 43 dpa. No damage of claddings made of ChS-68 steel (20% cold worked) was observed, and ductility margin existed. Maximum depth of cladding corrosion was within 15 μm. Swelling rates of (U0.4Pu0.6)N and (U0.55Pu0.45)N were, respectively, ∼1.1% and ∼0.68% per 1 at.%. Gas release rate did not exceed 19.3% and 19%. Pattern of porosity distribution in the fuel influenced fuel swelling and gas release rates.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.