Abstract

The resistance spot welding is adopted to joint dissimilar alloys such as aluminum alloy 5052, and low carbon steel alloy 1008. In this work, the electrodes force 2100-2700 N, the welding current 7.5-10.5 KA, and welding time 10-20 cycle have been used. The relationships between the three parameters have been studied. The maximum tensile shear load of the aluminum alloy 5052-low carbon steel 1008 joint has been found equal to 2860 N for weld nugget diameter of 9 mm. The intermetallic compound layer (IMC) with 2-8 μm thickness with tongue-like has been appeared adjacent to the 1008 low carbon steel side, whereas a needle-shaped IMC layer adjacent to the aluminum alloy 5052 side