Abstract

ObjectivesTo characterize the behavior of three different polymeric agents before and after an erosive challenge on dentin permeability, to analyze their degradation in both conditions, and to analyze their degree of conversion (DC). MethodsThe permeability of human dentin disks (1.0 ± 0.2 mm) was measured with smear layer, after its removal, after treatment (LpTreat) with Gluma Desensitizer, PRG Barrier Coat (PBC) or Icon infiltrant (n = 11/group) and after exposure to citric acid (LpEro) (6%, pH 2.1, 1 min). The specimens were analyzed under a Laser Scanning Confocal Microscope (n = 2/group) and the products’ DC were calculated. Data were subjected to 2-way repeated measures ANOVA and post-hoc Bonferroni (permeability analysis), to paired t-test (for specimens treated with Icon) and to t-test (DC analysis) (α < 0.05). ResultsIcon showed the lowest LpTreat and LpEro values, while PBC and Gluma did not differ from each other under these conditions. Icon and PBC showed LpEro similar to a dentin with smear layer. Under the Laser Scanning Confocal Microscope, more deposits were noticeable on dentin after treating with PBC. Gluma presented the deepest penetration in dentin. The DC of PBC was the highest. SignificanceIcon caused the highest reduction on permeability values, followed by PBC and Gluma. PBC generated more deposits covering dentin and seemed to be more efficient after an erosive challenge. The association of a polymeric resin with inorganic ion-releasing fillers seem to be a great strategy to manage dentin hypersensitivity under erosive conditions.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call