In the blast furnace production process, the high iron content in the sludge produced by collecting, Iron can be used as recycled raw materials. Experimental study found that the use of magnetic roasting - weak magnetic iron powder method of recovering technology is feasible. The optimum conditions are: the grinding fineness is 87%, calcination temperature is 750 °C, roasting time is 25min, magnetic current is 1.5A under conditions to obtain a grade of 59% recovery rate of 79.3% iron ore .
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.