The test simple was taken from old tailing in Burma. The results of the chemical analysis and the phase analysis indicated that the grade of Lead was 2.84%, with the oxidation rate of 58.33% and the grade of zinc was 3.22%, with the oxidation rate of 16.56% in the old tailing. Through the research of the flotation separation test, the optimal grinding fineness (-0.044mm) was accounts for 73%. The optimum dosage of sodium sulfide was 1500g/t and the dosage of potassium dichromate was 600g/t. The separation effect of copper and lead was better, the ultimate concentration index: the grade of copper was 16.58% in the copper concentrate and the recovery was 56.18%. The grade of lead was 48.83% and the recovery was 96.67% in the lead concentrate.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.