Flotation technology without fluorite was studied to separate low-grade K-feldspar with quartz. It is shown in the results that qualified K-feldspar concentrate can be gained by grinding, desliming, flotation and high intensity Magnetic Separation process. Feldspar concentrate obtained in closed-circuit had a content of K2O and Na2O 12.12%, quartz concentrate with a yield of 19.94% containing 97.12% SiO2 was obtained in the same time.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.