Abstract

The silicon-coated iron powder was evenly mixed with corundum powder and high temperature binder. After tabletting and sintering, followed by crushing and screening, the magnetic abrasive with a certain size was obtained. Scanning electron microscope (SEM), Energy dispersive spectrometer (EDS) and X-ray diffraction (XRD) were respectively used to characterize the morphology, elemental composition and the crystalloid structures of magnetic abrasive. The ferromagnetic phase and abrasive phase were combined firmly. The magnetic abrasive prepared showed a good grinding ability, whose durable time was up to 24 min. Irregular particles was obtained by smashing the magnetic abrasive, mainly composed of Al2O3, Fe2O3, α-Fe, AlFeO3, (Al, Fe)7BO3(SiO4)3O3.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.