Abstract

In this paper, Kenaf bast fiber were the research objective. The fiber morphology was studied, as well as the compatibility between fibers and cemented. At last. The manufacture technology for fiber reinforced cement-based panel was studied. The results are as follows: The average length of Kenaf bast fiber, which determines Kenaf bast fiber as long fibers. Effects of the influences of fiber to cement (w/c), water to cement (m/c) were significant. When the conditions of the process were following that the ratio of wood-cement ratio was 0.22, water-cement ratio of 0.42, the Kenaf bast fiber-cement panel met the requirement of excellence (MOR = 14 MPa, MOE = 3900 MPa, TS = 1.26%) specified in GB/T 24312-2009.