Abstract
Recovering gold form arsenic bearing gold mine through floatation has always been an important research subject, the gold ore contains 2.40 g/t of gold and content of arsenic was 1.2% in Hebei, cannot achieve good product indexes, in order to improve the efficiency of resource use, lime was adopted to control the pH value of pulp, NaHSO3was added to inhibit the arsenic, the floatation of gold was carried out priority. The gold concentrate contain 65.63g/t with the recovery was 89.92% and the content of arsenic was only 0.07% after closed-circuit experiment, that results means the product indexes were improved greatly compare the field product now.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.