Abstract

The elastic recovery property of a novel poly(ester-imide-ether) (PEIE) was prepared from the 1, 4-butanediol (BD), poly(tetramethylene glycol) (PTMG1000) and imide dicarboxylic acid based on 1, 2, 4-benzenetricarboxylic (TMA) and aminobenzoic acid (PABA) was studied. The elastic recovery of the PEIE was studied in the fiber form. The influences of the draw ratio, temperature and heat treatment on elastic recovery were investigated. The results show that the novel PEIE possesses the excellent elastic recovery at low temperature and the quickly-changed temperature is lower than that of traditional poly(ester-ether)s. Meanwhile, the heat treatment process can improve the elastic recovery of the PEIE because this process improves the crystallization of the hard segments.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.