Abstract

In order to investigate the corrosion behavior and impact toughness of 105SS drill pipe steel in the wet H2S environment, the impact and corrosion testing were carried out. The results show that the diffusible hydrogen concentration is mainly influenced by the morphology of the corrosion scales and the dynamic fracture toughness loss of 105SS drill pipe steels increases with the increase of diffusible hydrogen concentration. However, when hydrogen was released, the impact energy increases. The area of quasi-cleavage features on the fracture surfaces increases with the increase of hydrogen concentration.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.