Abstract

Residual stress produced on the surface of nanostructured ceramic coatings when they were grinded by diamond superhard abrasive wheel, these residual stresses affected directly the fracture strength, fatigue strength and corrosion resistance of the ceramic parts, they affected the surface quality of machined ceramic parts, and thus they affected the working reliability and the service life of ceramic parts. The tests show that the distribution of residual stress is directional, the residual compressive stress can make the hardness of the material increase, they can reduce the wear rate of the material, for the tested specimen, grinding surface whole residual stress σ is the sum up original residual stress σ0(existed in the part’s surface ) and grinding residual stress Δσ (formed by grinding process.), σ=σ0+ Δσ.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.