Mineralogical examinations of Asheler copper mine flotation tailings have been carried out. Results show that the major metal sulphide minerals are pyrite and the main gangue constituents are quartz, chlorite-serpentine and muscovite. The main valuable metals are Cu, Zn and Ag. Basic mineral compositions of copper and zinc have been identified through chemical phase analysis. On the basis of mineralogical examinations, leaching test has been carried out in about 240g/l NaCl solution. The optimum conditions for leaching are found as follows: temperature at 86°C, pulp concentration is 24.19%wt, [Cu2+] =19.22g/l, [HCl] initial =0.17mol/L. Under these conditions, chloride leaching can extract 83.35%Cu, 92.10%Zn, and 85.26%Ag after 8 hours leaching.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.