The results of the research on establishing the dependence of the coercive force (Нs) on special boundaries in a low-carbon alloy are given. Annealing at a temperature of 900 ºС with a holding time of 1 to 3 h leads to an increase in the number of special boundaries from 22.7 to 37.17% and to an increase in magnetic permeability and, accordingly, a decrease in the coercive force from 1.60 to 1.24 A/cm. When the load is axially stretched, the coercive force changes. The initial stage of plastic deformation is most sensitive to the growth of coercive force, which allows us to identify areas in which local plastic deformation has occurred, which indicates a significant decrease in the operational characteristics of parts.