Abstract

The influence of the concentration of the initial solution on the size and composition of the particles obtained by the method of ultrasonic spray pyrolysis (USP) was investigated. An aqueous solution of Fe (NО3)3·9Н2О, the concentration of which varied in the range of 0,0025–0,03 mol/l, was used as the starting material. As a result of the process, iron oxide particles were obtained, the average size of which varied from 123 to 292 nm. Based on FTIR and XRD, powders consist of several phases and have crystalline inclusions α-Fe2O3, β-Fe2O3, and γ-Fe2O3.