The effect of firing temperature on shrinkage or growth indices, porosity, and ultimate strength in bending is studied in specimens prepared from bauxite HCBS, and also additionally containing reactive alumina CTC-30. For all material compositions there are typical preferred sintering temperature ranges (900 – 1200°C) with prevalent mullitization accompanied by an increase (1200 – 1400°C) in sintering or shrinkage of mullitized material (1400 – 1600°C).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.