Abstract

We have studied the magnetic excitations in impurity doped La$_{1.85}$Sr$_{0.15}$Cu$_{1-y}$A$_{y}$O$_{4}$ (A=Ni or Zn) by neutron scattering. The dispersion for Zn:$y=0.017$ is similar to that for the impurity free sample: incommensurate peaks with the incommensurability $\delta=0.12\pm0.01$ (rlu) do not change their positions up to 21 meV. On the other hand, for Ni:$y=0.029$, two incommensurate peaks observed at low energies suddenly change into a broad commensurate peak at $E_\mathrm{cross}=15$ meV. Compared to the impurity free sample with a similar Sr-concentration $x=0.16$, [B. Vignolle {\it et al.} Nature Physics {\bf 3} (2007) 163], $E_\mathrm{cross}$ for Ni:$y=0.029$ is decreased by nearly the same factor for the reduction in $T_{c}$. This is very similar to the shift of the resonance energy ($E_\mathrm{res}$) in Ni-doped YBa$_{2}$Cu$_{3}$O$_{7}$.[Y. Sidis {\it et al.}: Phys. Rev. Lett. {\bf 84} (2000) 5900]. These common impurity effects on the shift of $E_\mathrm{cross}$ and $E_\mathrm{res}$ suggest the same magnetic origin for the resonance peak in YBa$_{2}$Cu$_{3}$O$_{\delta}$ and that for a crossing point of upward and downward dispersions in the La$_{2-x}$Sr$_{x}$CuO$_{4}$. We propose that the sudden change in the dispersion is better described by a crossover from incommensurate spin fluctuations to a gapped spin wave rather than a hourglass-like dispersion.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.