Abstract
AbstractThe reliability of oxide‐semiconductor (OS) thin‐film transistors (TFTs) is significantly influenced by the gate insulator (GI). During electrical bias stress, the defect sites near the semiconductor/GI interface and/or within the GI may trap electrons, which makes the threshold voltage (Vth) shift toward positive values. On the other hand, carbon (C) or hydrogen (H) atoms may diffuse from the GI into the active layer, and act as shallow donors, which induce negative Vth shifts (ΔVth). In this paper, an in situ atomic layer deposition (ALD)‐based GI heterostructure is introduced, which consists of a stack of two complementary materials, namely Al2O3 and SiO2. Here, a competition occurs between electron trapping in Al2O3 (positive ΔVth) and carrier generation from H atoms in SiO2 (negative ΔVth) which allows the achievement of nearly zero ΔVth under positive bias temperature stress (PBTS). This strategy is successfully applied to a high‐mobility (>50 cm2 Vs−1) ALD‐based indium‐gallium‐zinc oxide (IGZO) device, resulting in a net ∆Vth of −0.02 V under PBTS and drain current variation (∆ID) of +0.49% under constant current stress (CCS). The application of an in situ ALD process thus offers valuable insights to resolve the mobility versus reliability trade‐off in high‐performance oxide TFTs.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.