Abstract

The high chemical durability of iodine-bearing apatite phases makes them potentially attractive for immobilizing radioactive iodine. Reactive spark plasma sintering provides a dense ceramic as a wasteform. A design-of-experiments (DOE) approach was adopted to identify the main process/material parameters and their first order interactions in order to specify experimental conditions guaranteeing complete reaction, relative density of the wasteform exceeding 92% and the largest possible grain size. For a disposal of the wasteform in a deep geological repository, these characteristics allow minimization of the iodine release by contact with groundwater. It was found that sintering at a temperature of 450°C with an initial specific surface area of 3.3m2g−1 for the powder reactants is sufficient in itself to achieve the targeted characteristics of the wasteform. However, this relies on a liquid sintering regime the efficiency of which can be limited by the lead iodide initial content in the mix as well as by its particle size.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.