Abstract
AbstractResults from a series of tests intended to study loss of pretension force in bolted assemblies are presented. The test matrix included ASTM A325 assemblies with various direct tension indicators (DTIs), some through-hardened and some not, as well as assemblies without direct tension indicators. Bolt length and diameter and grade of nut were also varied. Load losses were monitored for 42 days (1,000 h). However, load levels generally stabilized after 14 days. Pretension losses were linearly dependent on initial pretension and not affected by DTI or washer configuration. Bolt diameter and length did affect the magnitude of losses over time but not the general linear relationship with initial pretension.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.