Abstract

The factors that affect the relation between ultimate tensile strength σu and hardness HB of gray cast iron with flaked graphite are studied. The scatter of the ultimate tensile strengths at a given hardness is shown to be caused by one of the primary structure parameters, namely, the volume fraction of primary austenite dendritic crystals. The dependences derived in this work can be used to increase the accuracy of a rapid estimation of the quality of cast iron ingots.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.