Abstract

This study evaluated the effect of short glass fibers on the transverse strength of a heat-polymerized acrylic resin denture base material. Four groups of specimens (n = 10) were fabricated according to the ISO standard for the transverse strength test. E-glass fibers were triturated to produce short fibers of different lengths. Specimens for Group 1 (control) were made of unfilled polymethylmethacrylate (PMMA). For group 2, the PMMA powder was modified with 0.1 g of dry glass fibers. For group 3, the PMMA powder was modified with 0.1 g of silanized glass fibers. For group 4, the PMMA powder was modified with 0.2 g of silanized glass fibers. A three-point loading test was used to determine the transverse strength of the tested specimens. The fracture surface of each specimen was evaluated using SEM. The addition of untreated glass fibers increased the transverse strength by 11% but produced some porosity in the polymeric matrix. The addition of silane-treated glass fibers increased the transverse strength of PMMA by 28% for group 3 and by 26% for group 4, and produced a dense structure for the polymer-fiber composite. The transverse strength of PMMA can be slightly increased by the addition of short glass fibers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.