Abstract

This investigation presents an experimental and analytical study on the behavior of reinforced concrete deep beams before and after repair. The original beams were first loaded under two points load up to failure, then, repaired by epoxy resin and tested again. Three of the test beams contains shear reinforcement and the other two beams have no shear reinforcement. The main variable in these beams was the percentage of longitudinal steel reinforcement (0, 0.707, 1.061, and 1.414%). The main objective of this research is to investigate the possibility of restoring the full load carrying capacity of the reinforced concrete deep beam with and without shear reinforcement by using epoxy resin as the material of repair. All beams were tested with shear span-depth ratio 2.2. An analytical study was made to show the behavior of a sample of test beam at higher stages of loadings before and after repair. The test results showed that the epoxy resin used for repairing was very efficient in restoring full capacity of failed beams. Moreover, epoxy resin increased the strength capacity of the original beams by about 14% to 40%. On the other hand, the increase in the longitudinal reinforcement increased significantly the ultimate capacity of deep beams before and after repair.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.