New types of potent aprotinin-containing medicinal polymer films are elaborated for topical applications. The higher the temperature of drying, the lower the steam absorption, the film swelling, and the velocity of aprotinin in vitro release. The presence of antimicrobials having the basic functional groups contributed to compacting the structure of the films and retention of aprotinin in them. The velocity of aprotinin release from the films is regulated by adding different polymers. Inclusion of polyvinylpirrolidone in the film resulted in acceleration and increase of aprotinin release. This was probably because of increasing the film swelling by a factor of 1.7. Additional retention of the inhibitor in films was achieved by inclusion of sodium alginate and cellulose powder capable of binding aprotinin. Soluble bioadhesive films derived from a copolymer of acrylamide, N-vinyl-pirrolidone, ethyl acrylate (M r 30,000-600,000) and aprotinin were obtained and analyzed. Kinetics of aprotinin release from biosoluble films was studied under various conditions. The duration of aprotinin release was comparable with duration of gradual dissolution of the matrix. Bioavailability of aprotinin from soluble films was linear with time.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.