Abstract

For the purpose of reduction of polyethylene wear generated in artificial hip joints, concave dimples were formed on the surface of the metal femoral head by electrical discharge etching with the constant diameter of 0.5 mm, pitch of 1.2 mm, and depth of 0.1 mm. Using a hip joint simulator, the total amount of polyethylene wear was 7.2 mg in the concave-patterned condition and 23.1 mg in the nonpatterned condition. The reasons for the reduction of polyethylene wear by the concave pattern may be i) a reduction of abrasive wear by providing escape dimples for wear particles and ii) an improvement in the lubricity on the frictional surface by the supply of lubricant that is stored in dimples.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.