The possibility of fracture reduction as a result of application of specific surfactants during intensive drying of clay-like materials was examined in this paper. The dodecyl sulfate sodium salt (SDS) and the fluoric (FC 4430) surfactants were used for the tests. Different amounts of these surfactants were mixed with distilled water and used for wetting a dry clay material before forming clay samples. The clay samples in the form of cylinders 44mm in diameter and 50mm high were extruded and after leveling the moisture distribution subjected to convectively drying in hot air at 120°C. The acoustic emission (AE) method was used to monitor on line the development of crack formation in dried samples. It was stated that application of surfactants in a prescribed amount may significantly reduce the drying induced fractures in clay during its intensive drying and thus to obtain good quality products by high drying rates.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.