Abstract

Reducing thermal contact resistance (TCR) is an important way to enhance heat dissipation of electronic devices. Elastomer is easy to deform, increase the contact area and reduce the TCR, but its wetting condition is not satisfying. In this work, a novel elastomeric thermal interface materials (TIMs) polyethylene glycol/unsaturated polyester resin/graphene (PEG/UPR/G) was designed and prepared. With the increase of temperature, PEG near surface of PEG/UPR/G was released due to phase transformation, and a thin molten layer would be attached to the surface. By this way, the micro bumps on the solid surface were all soaked by the thin layer of molten PEG, which greatly reduced the TCR. In addition, the effect of temperature and pressure on TCR of elastomeric PEG/UPR/G were studied. When the pressure increases from 10 Psi to 50 Psi (65 °C), TCR decreases from 11–14 K ∙ cm2/W to 2–4 K ∙ cm2/W. The TCR will be further reduced to 0.7–0.9 K ∙ cm2/W (75 °C) due to the phase transition of PEG. Moreover, the heat dissipation effect of PEG/UPR/G was evaluated by infrared thermal imager. These results demonstrate that the total thermal resistance is the decisive factor for the final steady-state temperature and the time of unsteady heat transfer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.