Abstract
A mineral carbonation method for using anthropogenic carbon dioxide emissions is discussed. In this method, steel manufacturing slags are carbonated with gaseous carbon dioxide at atmospheric pressure and temperature using an aqueous ammonium chloride solution. This lixiviant extracts calcium selectively from the slag material, after which the dissolved calcium is precipitated as calcium carbonate. A flue gas stream can be used as a CO2 source without pre-separation. The reactions occur pseudo-catalytically in one vessel, resulting in considerable savings regarding process capital costs and reagent usage compared to a previously developed two-step carbonation method (Slag2PCC). The one-step method uses steel slag more efficiently, potentially reducing the amount of landfilled slag while capturing significantly more carbon dioxide in the same amount of slag. The two-step method produces >95% pure calcium carbonate, which can be used, e.g., in papermaking, while the one-step method is capable of manufacturi...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.