KY(WO4)2 is a promising material for on-chip laser sources. Deep etching of small KY(WO4)2 samples in combination with various thin film deposition techniques is desirable for the manufacturing of such devices. There are, however, several difficulties that need to be overcome before deep etching of KY(WO4)2 can be realized in small samples in a reproducible manner. In this paper, we address the problems of (i) edge bead formation when using thick resist on small samples, (ii) sample damage during lithography mask touchdown, (iii) resist reticulation during prolonged argon-based inductively coupled plasma reactive ion etching (ICP-RIE), and (iv) redeposited material on the feature sidewalls. We demonstrate the etching of 6.5 µm deep features and the removal of redeposited material using a wet etch procedure. This process will enable the realization of waveguides both in ion-irradiated KY(WO4)2 as well as thin KY(WO4)2 membranes transferred onto glass substrate by bonding and subsequent polishing.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.