1 cm ×12 cm rectangular YBCO films for fault current limiter devices were prepared by MOD. Usually, solution coating in MOD is carried out by spin coating. However, there are some problems associated with spin coating of large-size rectangular substrates. Namely, the maximum substrate dimension is limited by cup size and motor torque of the apparatus. It was found that wire-bar coating is a promising alternative; this method is more easily scaled up to a large size at lower cost. By both methods, YBCO films with high Jc's around 2 MA/cm2 were obtained on CeO2-buffered sapphire. So far, the uniformity of Jc in the YBCO films prepared by spin coating was better than those by wire-bar coating.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.