Abstract

1. An increase of the initial recrystallization temperature of electrolytic iron as compared with pyrometallurgical iron is due to the large amount of oxygen and oxygen-containing impurities in the metal, which pin dislocations and inhibit the formation of recrystallization nuclei. 2. With increasing initial hardness of the coating the initial recrystallization temperature and the grain size increase.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.