Abstract

In this study, recovering of zinc ions in the residual solution occurring after copper cementation by zinc metal was investigated. The zinc ions in the solution were recovered by using sodium bicarbonate as precipitation agent. After the precipitated product was separated from the solution, it was dried at 80°C for 5 h in an oven and was subjected to the calcination process to obtain zinc oxide. The XRD and SEM analyses of the precipitated and calcined products were carried out. It was determined that the precipitated solid was Zn5(CO3)2(OH)6 (hydrozincite) and the calcined product was ZnO.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.