Abstract
A hydrometallurgical treatment involving solvent extraction of zinc using di-2-ethylhexyl phosphoric acid (D2EHPA) has been investigated to recover zinc from an industrial leach residue. The residue was leached with sulfuric acid producing leach liquor which was subjected to solvent extraction for enrichment of zinc and removal of impurities. Operating variables, such as pH, D2EHPA concentration, temperature, aqueous/organic (A/O) phase ratio, tri-butyl phosphate (TBP) concentration and sodium sulfate (Na 2SO 4) concentration in aqueous phase were studied. Practically, all zinc was extracted from the aqueous solution at pH 2.5 with 20% w/w D2EHPA in kerosene. Increasing either TBP concentration up to 5%, or Na 2SO 4 concentration up to 0.2 M, increased the zinc extraction. Zinc could be extracted at one theoretical stage at A/O of 1/1, as calculated by McCabe–Thiele method.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.