Abstract
Many attempts has been taken for further utilisation of the tailings and slimes through different routes i.e. beneficiation, agglomeration etc. Though the slimes and tailings contain huge ultra fines, conventional beneficiation methods many not be much effective for handling because of particle size limitations. Physicochemical method i.e. selective flocculation is a process for handling the ultrafine particles present in the tailings. Review shows that selective flocculation technique have very limited commercial application. Here the study focuses on the application of selective flocculation process for beneficiation of synthetic mixtures of iron ore and kaolinite as well as iron ore tailings. Results show that it is possible to achieve 65.78(%) of Fe, with 2.65% Al2O3, 3.66 SiO2 (%) in the concentrate using synthetic mixture feed and more than 60% of Fe is obtained from natural iron ore tailings.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.