Abstract This study is devoted to tellurium recovery from sodium carbonate slag, formed in the fire refining process of crude silver. The slag was modified by silica additions and then reduced by carbon oxide. The degree of the slag modification was defined by the parameter kw: where:ni- the mole numbers of silica, sodium carbonate and sodium oxide. The compositions of the investigated slag determined by the parameter kw and the mole fraction of the tellurium oxide (xTeO2 ) are given in the following Table. The reduction of tellurium was very fast for all the investigated slags, which was manifested by an almost complete conversion of CO into CO2. Unfortunately, at the same time, a side reaction took place, and as a results sodium telluride was formed, which reported to the slag: (Na2O)slag + Te(g) + CO = (Na2Te)slag + CO2 The tellurium content in the reduced slag decreases as the parameter kw increases, and only the slag with the kw equal unity was suitable for the tellurium recovery in form of dusts, containing more than 76 wt-% tellurium.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.