Abstract

The recovery of iron from chromium vanadium-bearing titanomagnetite concentrate was investigated by direct reduction, followed by magnetic separation. The results indicated that the metallization rate of iron can reach 98.9% at a temperature of 1200°C for a reduction duration of 60 min with the addition of 16% graphite powder and 0.5% sodium oxalate. Although the addition of borax, sodium carbonate and sodium oxalate to the chromium vanadium-bearing titanomagnetite concentrate can all improve the metallization rate of iron, the effect of sodium oxalate was the best. Sodium oxalate not only increases the metallization rate of iron but also promotes the growth of metallic iron. After magnetic separating, the recovery of iron was 92.8% and the iron content of magnetic concentrate was 88.4%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.