Abstract

Two heavy metals, Cd and Ni, have been separately recovered from spent AA-size Ni–Cd batteries by the potentiostatic electrodeposition and chemical precipitation methods, respectively. Various types and concentrations of HCl, H 2SO 4, and HNO 3 acids had been used as leach extractants. Experimental results indicate that the acid with the best leach capability is 4 M HCl. Three complexing reagents of NH 3, sodium acetate, sodium citrate have been chosen and tested. The most effective buffer is sodium citrate. The optimum mole ratio of metallic ion to citrate ion is 1:1. The recovery process for Cd metal is conducted by the potentiostatic electrodeposition in a leach electrolyte with a sodium citrate complex. The optimum applied potential for Cd recovery is in the range −1100 to −1120 mV (versus saturated calomel electrode (SCE)). The current efficiency for the recovery process is between 70 and 90% and depends strongly on the process parameters, e.g. liquor, concentration, applied potential, temperature, type of complex reagents, mole ratio, mass-transfer rate.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.