Abstract The pretreatment of the cyanide tailing by roasting and its effect on the followed comprehensive recovery of valuable metals were investigated. The results indicate that the leaching rate of gold reaches 46.14%, the magnetic susceptibility of iron is up to 86.27% when the roasting temperature is 750 °C, the roasting time is 1.25 h, and the dosage of reductant is 6%. Combined with mineral structure and principle of magnetic roasting, the promoting mechanism of gold leaching by roasting was explored. The gold exposed through the magnetic roasting is the foremost improvement for high leaching rate of gold.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.