ABSTRACT Oxalic acid was used for recovering cobalt from leaching solution of spent lithium ion battery by precipitation method. Crushed powders containing LiCoO2 of spent lithium ion battery were obtained by crushing, magnetic separation and screening process. These powders were dissolved in 2 M H2SO4 solution with H2O2 as a reducing agent. After dissolving Co and Li components, the solution of oxalic acid was added. Co(II) in leaching solution could be removed in the form of insoluble oxalates. The precipitate formed was crystalline, compact and easily filtered. With the increase in oxalic acid, the rate of cobalt precipitate increased to 90% at 1:4 mole ratio of Co(II) and oxalic acid concentration. When cobalt ion was precipitated into cobalt oxalate, nickel and copper ions were co-precipitated but there were no co-precipitates of Li, Al and Fe. The amounts of Ni and Cu in the solutions were below 1%. After heat treatment of precipitates at above 250°C, cobalt oxalate was changed into cobalt oxide.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.