Abstract

The aluminum electrolysis industry continually and unavoidably produces hazardous solid waste in the form of carbon anode slag. Carbon anode slag poses a serious environmental pollution risk, and it must be disposed of in a harmless manner. On the other hand, it contains a few valuable resources, as well. In order for the aluminum electrolysis industry to develop in an environmentally friendly and high-quality manner, the harmless disposal of carbon anode slag and its resourceful utilization are of considerable importance. The selective comminution of carbon and cryolite particles in carbon anode slag can be effectively achieved with grinding pretreatment. However, the optimization study of grinding process parameters has yet to be investigated. Therefore, firstly, the mineralogical characteristics and existing mode of carbon anode slag from the perspective of mineralogical properties are analyzed in this study. Then, the effects of grinding time, grinding concentration, and steel ball diameter on the particle size of the ground product (γ−0.074 mm) are investigated using response surface analysis. The results showed that the effect of grinding time was the most significant, followed by grinding concentration and steel ball diameter. In addition, the performance of the multi-stage flotation process for separating the −0.074 mm ground product was analyzed. Cryolite with a purity of 93.12% and a carbon product with an ash content of 10.67% could be simultaneously obtained through multi-stage flotation. It should be pointed out that the deep dissociation and efficient recovery of fine undissociated particles still need to be further explored.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call