Abstract
Sulfur-cured filled natural rubber (NR) is successfully reclaimed by using a renewable resource material (RRM) and diallyl disulfide (DADS), which is the major constituent of RRM. Reclaiming of NR vulcanizate was carried out at 60°C for 35 min in an open two-roll mixing mill. Evaluation of the properties of NR reclaim was carried out by mixing it with virgin rubber in various proportions. The cure characteristics and mechanical properties of the virgin NR/ reclaim NR blend were studied. With increase in the proportion of reclaim rubber (RR) in virgin NR/ reclaim NR blend scorch time and optimum cure time decrease. To increase scorch time N-cyclohexylthiophthalimide as prevulcanization inhibitor (PVI) was added in NR/RR (50/50) blend. It was found that use of 40% NR reclaim with virgin rubber resulted 83% retention of tensile strength of that of the virgin NR vulcanizate. Effect of carbon black loading was studied in NR/RR (50/50) blends. Tensile properties and swelling value of different NR/RR blends were evaluated before and after aging. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 75: 1493–1502, 2000
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.