Abstract

The Paton Welding Journal, 2014, №03. International Scientific-Technical and Production Journal «The Paton Welding Journal» «The Paton Welding Journal» has been published monthly since 2000 in English, ISSN 0957-798X. «The Paton Welding Journal» is a cover-to-cover English translation of the «Avtomaticheskaya Svarka» (Automatic Welding) journal. The «Avtomaticheskaya Svarka» journal has been published monthly since 1948 in Russian, ISSN 005-111X.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.