Poly(ethylene terephthalate) (PET) was blended with polystyrene (PS) and poly(styrene-co-maleic anhydride) (PScMA). The two blend systems were immiscible based on the glass transition temperatures measured by differential scanning calorimetry (DSC). In the case of 70 and 90% PScMA blends, the reaction between ester groups of PET and maleic anhydride (MAH) sites on PScMA occurred during melt mixing at 280°C for 30min. The reaction was confirmed indirectly by thermal data, from the increase in the complex viscosity and from the solubility difference between the blends. The particle size in PET/PScMA reactive blends was smaller than that of the non-reactive blends. The mechanical properties such as tensile strength and modulus were not affected by the reaction.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.