The new joining method of SiC components with channel was developed in this study by using hot-press. The SiC ceramics was joined by using mixed Al 2O 3, Y 2O 3, SiO 2 and SiC powders. Joining was carried out at from 1500 °C to 1900 °C for 1 h, under an applied pressure, range from 5 MPa to 20 MPa. Microstructural characterization was carried out for the joined materials by optical and scanning electron microscopy. The mechanical property of the joint was evaluated through a tensile test. The joint strength was increased with increasing joining temperature and pressure. In joining of complex shape SiC components, the serious deformation of substrate occurred because of high joining temperature and pressure. The low joining condition, In case of 1800 °C and 20 MPa, deformation of substrate not occurred. It is possible that the deformation of substrate was controlled by joining temperature. The joint layer of SiC component by using new joining method was cleaned and uniformed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.