Abstract
Model composites consisting of SiC fiber and Yb2SiO5 were processed by the spark plasma sintering (SPS) method. The mechanical compatibility and chemical stability between Yb2SiO5 and SiC fiber were studied to evaluate the potential application of Yb monosilicate as the interphase of silicon carbide fiber reinforced silicon carbide ceramic matrix composite (SiCf/SiC CMC). Two kinds of interfaces, namely mechanical and chemical bonding interfaces, were achieved by adjusting sintering temperature. SiCf/Yb2SiO5 interfaces prepared at 1450 and 1500 °C exhibit high interface strength and debond energy, which do not satisfy the crack deflection criteria based on He-Hutchison diagram. Raman spectrum analyzation indicates that the thermal expansion mismatch between Yb2SiO5 and SiC contributes to high compressive thermal stress at interface, and leads to high interfacial parameters. Amorphous layer at interface in model composite sintered at 1550 °C is related to the diffusion promoted by high temperature and DC electric filed during SPS. It is inspired that the interfacial parameters could be adjusted by introducing Yb2Si2O7−Yb2SiO5 interphase with controlled composition to optimize the mechanical fuse mechanism in SiCf/SiC CMC.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.